Honeywell XNX Stainless Steel vs. Aluminum Body: AMSV vs. AMAI vs. AMAV Corrosion Ratings
Honeywell’s XNX transmitter family ships in three aluminum-body variants (AMAI, AMAV, AMAR) and one stainless-steel-body variant (AMSV). The material choice is permanent at the factory — you cannot field-swap an AMAI body for an AMSV body. That means corrosion-risk misjudgment during ordering can condemn a $1,800 transmitter to failure in a coastal environment within months.
The Four Variants
| Variant | Body Material | Certification | Temperature | Impact Rating | Primary Use |
|---|---|---|---|---|---|
| XNX-AMAI | Aluminum die-cast | ATEX II 2G Ex d IIC T4 Gb | –40 °C to +75 °C | IK08 / 5 J | Inland refineries, process plants |
| XNX-AMAV | Aluminum die-cast | Same as AMAI | Same | Same | Older production; V and A are equivalent |
| XNX-AMSV | 316 stainless steel | Same as AMAI | –50 °C to +85 °C | IK10 / 20 J | Offshore, coastal, marine, heavy-chloride |
| XNX-AMAR | Aluminum die-cast | Same as AMAI | Same | Same | AMAI variant with relay option at factory |
Salt-Spray Corrosion Test (ASTM B117)
| Body | ASTM B117 Survival | Penetration Resistance | Surface Treatment |
|---|---|---|---|
| Aluminum AMAI / AMAV | < 200 hours | Pitting at screw holes within 3 months | Passivation + powder coating |
| Stainless 316 AMSV | > 500 hours | No red rust; some crevice pitting at 1000 h | Passivated, no coating |
Chloride concentration rule of thumb: if your site sees > 3 ppm chloride in process water or is < 100 m from a saltwater coastline, order AMSV stainless. Aluminum is fine at < 3 ppm and > 1 km inland.
Temperature Range
| Body | Min Temp | Max Temp | Reason |
|---|---|---|---|
| Aluminum AMAI / AMAV | –40 °C | +75 °C | Powder coating degrades above 80 °C; galvanic corrosion accelerates |
| Stainless AMSV | –50 °C | +85 °C | 316 SS stable to +250 °C; rating limited by electronics |
XNX-30 IR caveat: even AMSV bodies cannot operate above +55 °C with the IR CO₂ sensor mounted directly on the body — the IR window has a +55 °C thermal limit. Use the XNX-30-REMOTE kit for hot areas.
Impact Resistance
The XNX bodies are explosion-proof pressure vessels — a crack means loss of ATEX certification.
| Body | IK Code | Drop Impact | Resisted Event |
|---|---|---|---|
| Aluminum AMAI / AMAV | IK08 | 5 J | Tool dropped from 1 m |
| Stainless AMSV | IK10 | 20 J | Pipe wrench strike, 2 m drop |
Offshore platforms where tool-drops are routine and consequence is catastrophic — AMSV stainless is mandatory.
How to Order the Right Body
The 5th segment of the part number tells you the material:
– A (AMAI / AMAV / AMAR) → Aluminum
– S (AMSV) → Stainless steel 316
Decision tree:
- Is your site < 100 m from coastline or chloride > 3 ppm? → AMSV
- Is ambient temperature > 75 °C or < –40 °C? → AMSV
- Is impact risk high (offshore, construction, mining mobile)? → AMSV
- Otherwise → aluminum AMAI / AMAV (lower cost, sufficient for process plant interiors)
Can You Retrofit a Damaged Aluminum Body?
No. The body is the primary pressure vessel for the explosion-proof rating. Honeywell does not sell replacement bodies — a cracked AMAI / AMAV requires full transmitter replacement. Internal spare parts (sensor heads, relays, HART adapters, fuse F1) are available and interchangeable between AMAI and AMSV bodies — the sensor head, HART module, and relay board are identical electronics.
Inventory of Both Types
We stock AMAI-NNNN (aluminum) and AMSV-NNNN (stainless) body units in multiple quantities. Contact us with your part number and environment description — we’ll confirm you picked the right body before you order, since switching after purchase means buying a new transmitter.
For the complete XNX fault code reference — F-00 to F-127, all mA states — jump to our master fault code hub.
Related Guides
- XNX-AMAI-NNNN Order Code Breakdown — segment-by-segment meaning
- XNX-AMSV-NNCB1 Stainless Catalytic Bead — stainless body + CB1 sensor configuration
Frequently Asked Questions
Can I use an aluminum AMAI body in a coastal oil terminal?
No — unless the terminal is at least 1 km inland and chloride concentrations are < 3 ppm. ASTM B117 shows AMAI aluminum develops penetrating red rust at screw holes and cable glands within 200 hours of 5 % NaCl mist — in a coastal terminal that translates to approximately 3–6 months of real service before the explosion-proof seal is compromised. AMSV stainless is mandatory.
What do I do if I ordered AMAI aluminum but my site has high chloride?
Three options: (1) Return the unused transmitter to Honeywell for a same-config AMSV exchange within 90 days — most distributors allow this, (2) Use the AMAI only in the lowest-chloride zone (indoor control room), (3) Order the correct AMSV transmitter immediately and cancel deployment. Do not try to make it work with protective coatings — they trap salt moisture against the body and accelerate corrosion.
Is the internal electronics different between AMAI and AMSV bodies?
No. The PCB, J304 sensor connector, HART module, power supply, and relay board are all identical. Only the external body material and its explosion-proof pressure rating differ. This means sensor heads (CB1, EC NH₃, XNX-30 IR CO₂), relay modules, HART adapters, and POD kits are 100 % interchangeable between AMAI and AMSV bodies.